Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434. EASTALLOY DA003-8999K Polymer is a clear copolyester/polycarbonate alloy. It has excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhanced physical properties advantages.
Applications: Medical
All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness.
Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given. Information provided by Eastman Chemical. |