MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Michelman® Hydrosize® U5-01 Polyurethane dispersion
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Description: Polyurethane dispersion

Usage: Hydrosize® U5-01 is a specialty coating and fiber sizing which offers improved thermal stability, higher strength and elongation to break

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 - 1.15 g/cc1.00 - 1.15 g/cc
Volatiles 41 - 45 %41 - 45 %
pH 6.5 - 8.56.5 - 8.5
Brookfield Viscosity 50 - 1000 cP50 - 1000 cPSpindle # 3, rpm 60
 
Descriptive Properties
AppearanceMilky white liquid
Emulsifier ChargeAmine dispersed
Solids TypePolyurethane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials Disperbond® D31S Thermoplastic Polyurethane
Covestro Desmopan® 3385A Polyurethane
Avient Teslart™ PUD-1 ICP/Aqueous Polyurethane

WMICHEL035 / 134952

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.