MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Teslart™ PUD-1 ICP/Aqueous Polyurethane  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes:
  • A dispersion of Teslart Inherently Conductive Polymer and an aqueous polyurethane binder.

Applications:

  • Designed as a starting point for formulation for formulators requiring a conductive coating
  • Anti-fouling Marine Coatings
  • Antistatic Fabrics, Coatings and Packaging
  • Batteries
  • Conductive Inks and Adhesives
  • EMI/RFI Shielding
  • Radar / Microwave Absorption and Sensors

Custom dispersions can be created to meet a desired surface resistivity value or other physical characteristics.

Disclaimer: Material should remain sealed in storage. Avoid freezing.
Teslart ICP's are made under license of NASA.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccCalculated
Solids Content 25 - 36 %25 - 36 %
pH 1.5 - 5.01.5 - 5.0
Brookfield Viscosity 125 cP125 cPLVT #2, 60 RPM
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1000 - 1.00e+10 ohm1000 - 1.00e+10 ohm4 Point Probe
 
Descriptive Properties
Active Ingredient0 to 25%Lignosulfonic acid grafted polyaniline wetcake
Binder/Vehicleaqueous polyurethane
ColorGreen / Black
Product FormLiquid

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Michelman® Hydrosize® U5-01 Polyurethane dispersion
Lubrizol Advanced Materials Disperbond® D31S Thermoplastic Polyurethane
Covestro Desmopan® 3385A Polyurethane

PH1PO3344 / 45020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.