MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Bergamid™ B70 G/GK30 TM-Y UV NC Polyamide 6 (Nylon 6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/cc±0.03; ISO 1183
Filler Content 30 %30 %Glass Bead\Glass Fiber
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 4.00 mm,
Temperature 23.0 °C
0.0040 - 0.0080 in/in
@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded, Bergmann Method; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 90.0 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
13100 psi
@Thickness 0.157 in,
Temperature 73.4 °F
5.0 mm/min; ISO 527
Elongation at Break 3.0 %
@Thickness 4.00 mm,
Temperature 23.0 °C
3.0 %
@Thickness 0.157 in,
Temperature 73.4 °F
5.0 mm/min; ISO 527
Tensile Modulus 5.40 GPa
@Thickness 4.00 mm,
Temperature 23.0 °C
783 ksi
@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded; ISO 527-2/1
Flexural Strength 115 MPa
@Temperature 23.0 °C
16700 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 4.10 GPa
@Temperature 23.0 °C
595 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact Unnotched  5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
Injection Molded; ISO 179
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 179
Charpy Impact, Notched  0.650 J/cm²
@Temperature -30.0 °C
3.09 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohm1.00e+15 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 205 °C
@Thickness 4.00 mm
401 °F
@Thickness 0.157 in
Unannealed; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
@Thickness 4.00 mm
374 °F
@Thickness 0.157 in
Unannealed; ISO 75-2
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
ALL; Internal Method
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 280 °C464 - 536 °F
Mold Temperature 65.0 - 85.0 °C149 - 185 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
AppearanceNatural Color
FeaturesGood Dimensional Stability
 Good Impact Resistance
 Good Stiffness
 Good UV Resistance
FormsPellets
Generic MaterialNylon 6
Generic NamePolyamide 6 (Nylon 6)
Processing MethodInjection Molding
Regional AvailabilityEurope
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergamid™ A70 GK30 H Polyamide 66 (Nylon 66)
Envalior Akulon® Ultraflow K-FHG6 PA6-GF30, Dry, 30% Glass Filled, Heat Stabilized
Avient Bergamid™ A70 GK30 black 13539126 Polyamide 66 (Nylon 66)
RTP Company RTP 200 GB 30 HS Nylon 6/6 (PA), Glass Bead - Heat Stabilized
RTP Company RTP 200 GB 30  Nylon 6/6 (PA 6/6) Glass Bead 30%

PH0POL1453 / 146022

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.