MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Bergamid™ A70 GK30 H Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³±0.03 g/cm³; DIN 53479
Filler Content 30 %30 %Glass Bead
Ash 30 %30 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 - 90.0 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
8700 - 13100 psi
@Thickness 0.157 in,
Temperature 73.4 °F
depending on color; ISO 527-2/5
Elongation at Yield 2.5 - 4.0 %
@Thickness 4.00 mm,
Temperature 23.0 °C
2.5 - 4.0 %
@Thickness 0.157 in,
Temperature 73.4 °F
depending on color; ISO 527-2/5
Tensile Modulus 4.00 - 4.80 GPa
@Thickness 4.00 mm,
Temperature 23.0 °C
580 - 696 ksi
@Thickness 0.157 in,
Temperature 73.4 °F
depending on color; ISO 527-2/1
Charpy Impact Unnotched 0.250 - 0.420 J/cm²
@Temperature 23.0 °C
1.19 - 2.00 ft-lb/in²
@Temperature 73.4 °F
depending on color; ISO 179/1eU
Charpy Impact, Notched 2.50 - 4.00 J/cm²
@Temperature 23.0 °C
11.9 - 19.0 ft-lb/in²
@Temperature 73.4 °F
depending on color; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Strength 60.0 kV/mm1520 kV/inIEC 60243-1
Comparative Tracking Index 500 V500 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 261 °C502 °FISO 3146
Maximum Service Temperature, Air 110 °C230 °FContinuous (GTP 50% Tensile); IEC 60216
 220 °C428 °FShort Time; IEC 60216
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FUnannealed; ISO 75-2/A
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
UL 94
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
UL 94
 
Descriptive Properties
FeaturesHeat Stabilized
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
K-Value74.0 to 78.0No Standard; 96% H2SO4
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergamid™ B70 G/GK30 TM-Y UV NC Polyamide 6 (Nylon 6)
Avient Bergamid™ A70 GK30 black 13539126 Polyamide 66 (Nylon 66)
Avient Bergamid™ A70 G15 HW TM-Z Polyamide 66 (Nylon 66)
Avient Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer
BASF Ultramid® A3WG6 BK 00564 30% Glass Filled PA66 (Conditioned)

PH0POL1462 / 146031

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.