MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexane (C6H14)
Categories: Fluid; Solvent

Key Words: C6H14
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.6603 g/cc
@Temperature 20.0 °C
0.02385 lb/in³
@Temperature 68.0 °F
Viscosity 0.30 cP
@Temperature 25.0 °C
0.30 cP
@Temperature 77.0 °F
Molecular Weight 86.18 g/mol86.18 g/mol
Vapor Pressure  0.1000 bar
@Temperature 9.80 °C
75.00 torr
@Temperature 49.6 °F
 0.161645 bar
@Temperature 20.0 °C
121.244 torr
@Temperature 68.0 °F
Surface Tension 17.89 dynes/cm17.89 dynes/cmat 25°C; Gamma
 18.4 dynes/cm
@Temperature 20.0 °C
18.4 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 30.2500 bar22689.3 torr
Critical Temperature 234.48 °C454.06 °F
Critical Density 0.234 g/cc0.00845 lb/in³
Critical Molar Volume 368 cm³/mol22.5 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 1.891.89
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 151.8 J/g65.30 BTU/lbEnthalpy of fusion at normal melting point
Heat of Vaporization 334.8 J/g144.0 BTU/lbEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 2.268 J/g-°C0.5421 BTU/lb-°F
 1.659 J/g-°C
@Temperature 25.0 °C
0.3965 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.120 W/m-K
@Temperature 25.0 °C
0.833 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
 0.0234 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
0.162 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 260 °F
gas
 0.0354 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
0.246 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 440 °F
gas
 0.0487 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
0.338 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 620 °F
gas
Melting Point -95.35 °C-139.6 °FAt atmospheric pressure (760 torr)
Boiling Point 69.0 °C
@Pressure 0.101 MPa
156 °F
@Pressure 14.7 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.3751
@Temperature 20.0 °C,
Wavelength 589.3 nm
1.3751
@Temperature 68.0 °F,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter15.8366
Antoine's Vapor Pressure B Parameter2697.55
Antoine's Vapor Pressure C Parameter-48.78
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)110-54-3
Chemical FormulaC6H14
Critical Compressibility (Zc)0.26
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A738.3
Dynamic Viscosity Parameter B366.11
Henry's Law Constant (atm m3/mol)0.000343
Molar Heat Capacity (298K)143.002 J/mol-K
Molar Heat Capacity of Vapor a Parameter-4.4099
Molar Heat Capacity of Vapor b Parameter0.5816
Molar Heat Capacity of Vapor c Parameter-0.0003117
Molar Heat Capacity of Vapor d Parameter6.489E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1208
UV cut-off (nm)210

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
n-Heptane, C7H16
2-Methylbutane, C5H12
Acetylene, Ethyne, C2H2
Butane (C4H10)
Ethane, C2H6

VORG025 / 74536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.