MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Butane (C4H10)
Categories: Fluid; Solvent

Key Words: C4H10
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.5788 g/cc
@Temperature 20.0 °C
0.02091 lb/in³
@Temperature 68.0 °F
Molecular Weight 58.12 g/mol58.12 g/mol
Vapor Pressure 0.1000 bar
@Temperature -49.1 °C
75.00 torr
@Temperature -56.4 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 37.959 bar28472 torr
Critical Temperature 151.96 °C305.53 °F
Critical Density 0.228 g/cc0.00824 lb/in³
Critical Molar Volume 255 cm³/mol15.6 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 80.18 J/g34.49 BTU/lbEnthalpy of fusion at normal melting point
Heat of Vaporization 386.1 J/g166.1 BTU/lbEnthalpy of vaporization at normal boiling temperature
Thermal Conductivity  0.0164 W/m-K
@Pressure 0.100 MPa,
Temperature 26.9 °C
0.114 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 80.3 °F
gas
 0.0284 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
0.197 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 260 °F
gas
 0.0430 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
0.298 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 440 °F
gas
 0.0591 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
0.410 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 620 °F
gas
Melting Point -138.3 °C-216.9 °FAt atmospheric pressure (760 torr)
Boiling Point -0.500 °C
@Pressure 0.101 MPa
31.1 °F
@Pressure 14.7 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.3326
@Temperature 20.0 °C,
Wavelength 589.3 nm
1.3326
@Temperature 68.0 °F,
Wavelength 589.3 nm
Na D line

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Methane (CH4)
Nickel Aluminide, NiAl
n-Heptane, C7H16
Acetylene, Ethyne, C2H2
2-Methylbutane, C5H12

VORG003 / 74514

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.