Buckeye Polymers BP RPP 1010 T Polypropylene, 10% Mineral Filled
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 10% Talc Filler
Material Notes:
This Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resistance to some aggressive chemical agents.
Key Words:
PP
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.950
g/cc
0.0343
lb/in³
ASTM D792
Linear Mold Shrinkage
0.014
cm/cm
0.014
in/in
ASTM D955
Melt Flow
10
g/10 min
10
g/10 min
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
33.1
MPa
4800
psi
ASTM D638
Flexural Modulus
1.70
GPa
247
ksi
ASTM D790
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
102
°C
216
°F
ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled
Borealis MC55T1 Polypropylene Compound 10% Mineral Filled
Cossa Polimeri ESTAPROP KUR 1520 TG05 Polypropylene, 10% Mineral Filled
Overview of materials for Polypropylene with 40% Glass Fiber Filler
A. Schulman POLYFLAM™ FPP 1007F Talc Filled Homopolymer Polypropylene
PBUK00 / 27855
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.