MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Optigel® WH Clay Additive
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: OPTIGEL® WH is produced from natural, colloidal aluminum silicate by a unique process. The high purity and consistent viscosity of OPTIGEL® WH are made possible by our selective mining and rigid process control from the crude ore to the finished product. OPTIGEL® WH is thixotropic in nature. It is most beneficial when it is used in combination with other rheological additives to produce the desired rheological properties in a paint system. Suitable co-thickeners include cellulosics, alkali swellables, and urethane thickeners. OPTIGEL® WH is a very economical thixotrope. OPTIGEL® WH is a fraction of the cost of most cellulosic thickeners. OPTIGEL® WH contributes to excellent spray atomization properties.

Application:

  • Economical
  • Heat Stable
  • Chemical Stability with Co-Solvents
  • Shear Tolerant
  • Enzyme-Proof
  • Rapid Shear Recovery
  • Low High Shear Viscosity
  • High Low Shear Viscosity
  • Wide Ph Range Tolerance (6-12)

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.481 g/cc0.0174 lb/in³Loose
 0.721 g/cc0.0260 lb/in³Packed
Particle Mesh Size 325 Mesh325 Mesh95%
pH 9.0 - 10.59.0 - 10.5
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 8.0 %<= 8.0 %
 
Descriptive Properties
Color/FormOff White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Optigel® LX Clay Additive
BYK Optigel® CK Clay Additive
BYK Optigel® WA Clay Additive
BYK Optigel® WX Clay Additive
BYK Optigel® W724 Thickener

PBYK105 / 185102

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.