MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Optigel® WA Clay Additive
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: OPTIGEL WA, a specially selected, activated, and organically modified smectite product, that has high swelling capacity in water and shows a marked thixotropic thickening effect.

Application:

  • Emulsion paints
  • Liquid dish-washing detergents
  • Emulsion plasters
  • Fritts and glazes
  • Silicone resin-based exterior paints
  • Foundry washes
  • Water reducible paints
  • Textured coating

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.40 g/cc0.0867 lb/in³
Brightness 70 %70 %Elrepho R 457
Particle Mesh Size <= 325 Mesh<= 325 Mesh95%
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 10 %<= 10 %
 
Descriptive Properties
Bulking Value0.049 US gallons/pound
Color/FormWhite, free flowing powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Optigel® LX Clay Additive
BYK Optigel® CK Clay Additive
BYK Optigel® WH Clay Additive
BYK Optigel® WX Clay Additive
BYK Optigel® W724 Thickener

PBYK104 / 185101

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.