MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta NP500CR Epoxy Glass Laminate Sheet, NEMA G-10
Categories: Polymer; Thermoset; Epoxy

Material Notes: NP500CR consists of a glass fabric with a specially formulated epoxy resin system resulting in excellent electrical characteristics and superior physical properties at cryogenic temperatures (-270°C to 135°C operating temperature range). It has very low thermal conductivity and has been produced specifically for use in cryogenic applications.

Information provided by Norplex-Micarta

Key Words: Glass Fiber, Epoxy, Micarta, Cryogenic, NEMA G-10, ASTM D709 Type IV Grade G-10, MIL-I-24768/2 GEE, IPC 4101/20, IEC 60893-2-EPGC 201, NIST G10CR
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc
@Thickness 12.7 mm
1.80 g/cc
@Thickness 0.500 in
ASTM D792
Moisture Absorption 0.100 %
@Thickness 1.57 mm
0.100 %
@Thickness 0.0620 in
ASTM D570 Condition A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100
@Thickness 6.35 mm
100
@Thickness 0.250 in
ASTM D785
Tensile Strength  262 MPa
@Thickness 3.17 mm
38000 psi
@Thickness 0.125 in
CrossWise; ASTM D638 Condition A
 310 MPa
@Thickness 3.17 mm
45000 psi
@Thickness 0.125 in
LengthWise; ASTM D638 Condition A
Flexural Strength  448 MPa
@Thickness 1.57 mm
65000 psi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
 517 MPa
@Thickness 1.57 mm
75000 psi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
Flexural Modulus  16.5 GPa
@Thickness 1.57 mm
2400 ksi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
 18.6 GPa
@Thickness 1.57 mm
2700 ksi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
Compressive Strength 448 MPa
@Thickness 12.7 mm
65000 psi
@Thickness 0.500 in
Flatwise; ASTM D695 Condition A
Shear Strength 152 MPa
@Thickness 1.57 mm
22000 psi
@Thickness 0.0620 in
perpendicular; ASTM D732 Condition A
Izod Impact, Unnotched  6.41 J/cm
@Thickness 12.7 mm
12.0 ft-lb/in
@Thickness 0.500 in
CrossWise; ASTM D256 Condition E-48/50
 7.47 J/cm
@Thickness 12.7 mm
14.0 ft-lb/in
@Thickness 0.500 in
LengthWise; ASTM D256 Condition E-48/50
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.8
@Thickness 1.57 mm,
Frequency 1e+6 Hz
4.8
@Thickness 0.0620 in,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Dielectric Strength  26.0 kV/mm
@Thickness 1.57 mm
660 kV/in
@Thickness 0.0620 in
ASTM D149 Condition D-48/50
 26.4 kV/mm
@Thickness 1.57 mm
670 kV/in
@Thickness 0.0620 in
ASTM D149 Condition A
Dielectric Breakdown  50000 V
@Thickness 1.57 mm
50000 V
@Thickness 0.0620 in
ASTM D149 Condition D-48/50
 60000 V
@Thickness 1.57 mm
60000 V
@Thickness 0.0620 in
ASTM D149 Condition A
Dissipation Factor 0.025
@Thickness 1.57 mm,
Frequency 1e+6 Hz
0.025
@Thickness 0.0620 in,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Arc Resistance 100 sec
@Thickness 3.17 mm
100 sec
@Thickness 0.125 in
ASTM D495 Conition A
Comparative Tracking Index 150 V
@Thickness 3.17 mm
150 V
@Thickness 0.125 in
ASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
@Thickness 3.17 mm
5.56 µin/in-°F
@Thickness 0.125 in
IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 13.0 µm/m-°C
@Thickness 3.17 mm
7.22 µin/in-°F
@Thickness 0.125 in
IPC-TM 650-2.4.24
Transformation Temperature, Tg 115 °C
@Thickness 12.7 mm
239 °F
@Thickness 0.500 in
DMA
UL RTI, Electrical 130 °C266 °FUL Bulletin 746b
UL RTI, Mechanical with Impact 140 °C284 °FUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
HB
@Thickness 0.0620 in
 
Descriptive Properties
Bonding Strength2200[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type 304L Stainless Steel
ATI Allegheny Ludlum AL 36™ Electrical Alloy (Cryogenic and Bimetal) UNS K93600 or UNS K93603
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
G-10 Fiberglass Epoxy Laminate Sheet

PNORPM052 / 192809

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.