MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum ATI 36™ Electrical Alloy (Cryogenic and Bimetal) UNS K93600 or UNS K93603
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal

Material Notes: ATI 36 alloy is a nickel-iron alloy combining low thermal expansion properties up to about 200°C (~400°F) along with moderately high strength and good toughness down to -253°C (-423°F), the temperature of liquid hydrogen. These properties combined with good weldability and desirable physical properties make this alloy attractive for many applications requiring precise dimensional stability. In applications such as in LNG tankers and in transportation and storage vessels for liquefied gas, ATI 36 alloy is of great advantage due to the minimization of any strains in the material resulting from thermal contraction. The composition of ATI 36 alloy for cryogenic application is adjusted to achieve very low thermal expansion coefficient at low temperature. This alloy is also used extensively in the manufacture of bimetallic components for electrical and electronic industries. It is the low expansion material used in the cladding of high expansion alloys, such as UNS K92510 to make bimetallic thermostats.

Key Words: Specs: ASTM B-753; ASTM F-1684; MIL-I-23011
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.05 g/cc0.291 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7575Typical Annealed
Tensile Strength, Ultimate 462 MPa67000 psiTypical Annealed
Tensile Strength, Yield 261 MPa
@Strain 0.2 %
37900 psi
@Strain 0.2 %
Typical; Annealed
Elongation at Break 32 %32 %typical in 2"; Annealed
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000810 ohm-cm0.0000810 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  0.500 - 1.10 µm/m-°C
@Temperature 25.0 - 93.0 °C
0.278 - 0.611 µin/in-°F
@Temperature 77.0 - 199 °F
 2.00 - 2.70 µm/m-°C
@Temperature 25.0 - 260 °C
1.11 - 1.50 µin/in-°F
@Temperature 77.0 - 500 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.030 %<= 0.030 %
Carbon, C 0.0080 %0.0080 %
Cobalt, Co <= 0.35 %<= 0.35 %
Iron, Fe 63 %63 %
Manganese, Mn 0.30 %0.30 %
Molybdenum, Mo <= 0.020 %<= 0.020 %
Nickel, Ni 36 %36 %
Silicon, Si 0.15 %0.15 %
Sulfur, S 0.0010 %0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals NILO® Alloy 36 Low-Expansion Alloy
Carpenter Invar 36® Alloy, Cold Drawn Bars
Kinetics MIM F15 (Kovar™) Low CTE Alloy
Carpenter Super Invar 32-5
Schott BOROFLOAT® Borosilicate Float Glass

NLE36 / 17999

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.