MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zircar Refractory Composites RS-BN Coat BORON NITRIDE COATING
Categories: Ceramic; Nitride

Material Notes: ZRCI Boron Nitride Coating Type RS-BNCoat is a high temperature, anti-stick release agent/lubricant for glass forming, hot pressing, super-plastic forming of alloys and melting/casting of non-ferrous metals. Type RS-BNCoat forms a non-wetting, non-reacting layer with molten aluminum and magnesium and their dross. It is ideal for forming a barrier layer to protect metal, ceramic, or graphite substrates used for metal transport or casting operations. Type RS-BNCoat’s high electrical resistance and high thermal conductivity makes it useful as a protective coating on electrical heating elements. It is available in a paint or as an aerosol. The aerosol allows easy application of uniform, thin layers, and the acetone/alcohol based carrier assures fast drying. Type RS-BNCoat is useful to temperatures to 1816°C (3300°F) in inert and reducing atmospheres. In vacuum atmospheres, RS-BNCoat can be used to 1400°C (2552°F) before sublimation, and in oxidizing atmospheres, its use temperature is 1093°C (2000°F).

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/cc
pH 2.0 - 4.02.0 - 4.0Coating pH
Brookfield Viscosity 1050 cP1050 cP3/60
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1100 °C2010 °F
Maximum Service Temperature, Inert 1400 °C2550 °FVacuum
 1800 °C3270 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 12.0 Month>= 12.0 Month
 
Component Elements PropertiesMetricEnglishComments
BN 85 %85 %
 
Descriptive Properties
ColorWhite
Type of BinderAl2O3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-99-45 Refractory Sheet
Zircar Refractory Composites RS-A3 Refractory Sheet
Zircar Refractory Composites RS-99-60 Refractory Sheet
DWA 6091/SiC/20p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
DWA 6092/SiC/40p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)

CZRCI33 / 2896

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.