MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Stat-Tech™ PC-CB2/000 CR Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Stat-Tech™ PC-CB2/000 CR XP100827

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 - 1.23 g/cc1.19 - 1.23 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.2 - 72.4 MPa8010 - 10500 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 - 7.0 %3.0 - 7.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.07 - 3.45 GPa300 - 500 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 89.6 - 103 MPa13000 - 14900 psiASTM D790
Flexural Modulus 1.72 - 3.10 GPa249 - 450 ksiASTM D790
Izod Impact, Notched 0.370 - 0.530 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
0.693 - 0.993 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 - 10000 ohm-cm100 - 10000 ohm-cmASTM D257
Surface Resistance 1000 ohm - 1e+051000 ohm - 1e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 123 °C
@Thickness 3.18 mm
253 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 112 °C234 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 - 320 °C572 - 608 °F
Mold Temperature 90.0 - 110 °C194 - 230 °F
Drying Temperature 120 - 130 °C248 - 266 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
 
Descriptive Properties
FeaturesClean/High Purity
 Electrically Conductive
Filler / ReinforcementCarbon Nano Filler
FormsPellets
Generic MaterialPC
Generic NamePolycarbonate (PC)
Processing MethodInjection Molding
Regional AvailabilityAsia Pacific
UsesAerospace Applications
 Automotive Electronics
 Business Equipment
 Computer Components
 Connectors
 Electrical Housing
 Electrical/Electronic Applications
 Housings

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Novamid® 3010SR NAT PA66
Eastman Eastar GN125 Copolyester, Natural
Avient LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer
Mitsubishi Iupilon® GPX 2010PH Polycarbonate
Overview of materials for Polycarbonate, Molded

PH0POL1103 / 145672

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.