MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond UV15LV One Component, UV Curable Epoxy Based System
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond UV15LV is a high strength, low viscosity, epoxy based UV curable system for bonding, sealing and coating. It has low viscosity and it is widely used in a variety of applications where spin coating is required. It is also completely free of any oxygen inhibition. UV15LV will cure quickly and easily when exposed to a UV light source with a wavelength range between 320-365 nm, with the optimum at 365 nm. The energy required is typically 20-40 milliwatts per cm². The rate of cure depends upon the distance of the light from the material being cured, the thickness of the section and the intensity of the light source. It typically cures in thicknesses of a micron or less up to 0.001-0.015 inches in 15-30 seconds or less. Epoxy based UVs are described as having a “cationic” curing reaction. This kind of system will have lower shrinkage (1-2%) and higher temperature resistance than the majority of UV systems that cure by a “free radical” mechanism. UV15LV has excellent resistance to a wide variety of chemicals including water, acids, bases, fuels and many solvents. It features good physical strength characteristics and electrical insulation properties. UV15LV has great adhesion to a wide variety of substrates including plastics, glass and many metals. As is typical with UVs, it has excellent optical clarity and light transmission properties. Cationic systems, such as UV15LV, tend to have much higher temperature resistance than other UV type systems. Its glass transition temperature (Tg) with a straight UV cure is about 85°C and when post cured for 30 minutes at 125°C, the Tg is about 120° C. This post cure also enhances UV15LV’s chemical resistance. The service temperature range for this system is -80°F to +300°F. It is widely used for a variety of applications in the optical, optoelectronic, aerospace and related industries.

Product Advantages:

  • One component system; no mixing needed.
  • Very low viscosity, easily applied; ideal for spin coating.
  • No oxygen inhibition while curing.
  • Cationic curing system.
  • Superior temperature resistance, especially when post cured with heat.
  • Outstanding optical clarity; excellent light transmission.
  • High bond strength; excellent adhesion to surface treated metals, glass and many plastics.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 70 - 120 cP70 - 120 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 75>= 75
Tensile Strength at Break >= 34.5 MPa
@Temperature 23.9 °C
>= 5000 psi
@Temperature 75.0 °F
Tensile Modulus >= 1.72 GPa
@Temperature 23.9 °C
>= 250 ksi
@Temperature 75.0 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 3.25
@Frequency 60 Hz,
Temperature 25.0 °C
3.25
@Frequency 60 Hz,
Temperature 77.0 °F
Dissipation Factor 0.020
@Frequency 60 Hz,
Temperature 25.0 °C
0.020
@Frequency 60 Hz,
Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 - 60.0 µm/m-°C30.6 - 33.3 µin/in-°F
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
Glass Transition Temp, Tg 85.0 °C185 °Fwithout post cure
 120 °C248 °Fwith post cure
Shrinkage 1.0 - 2.0 %1.0 - 2.0 %
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5171.517
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in original unopened containers with no exposure to light

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP17HT-3 One component, snap-curing epoxy system
Master Bond UV22DC80-1 One component, nanosilica filled, dual cure epoxy
Master Bond UV22 One Component, UV Curable, Nanosilica Reinforced Epoxy System
Master Bond UV16 High Strength UV Curable Epoxy System

PMASTB329 / 149576

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.