MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilon® TSGK-30/4 X PA666-(GF+GB)30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Product description: Grilon TSGK-30 X/4 is a heat stabilized PA 66 + PA 6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30/4 X has the following important properties:
  • Good flow behavior
  • High weld line strength
  • Low warpage
Grilon TSGK-30/4 X is used typically for housing elements, relais bearers, axle spindle casings and applications which demand medium level of stiffness and low warpage.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³Dry; ISO 1183
Water Absorption 5.0 %5.0 %Sim. to ISO 62
Moisture Absorption 2.00 %2.00 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 80.0 MPa11600 psiConditioned; ISO 2039-1
 135 MPa19600 psiDry; ISO 2039-1
Tensile Strength at Break 60.0 MPa8700 psiConditioned; ISO 527-1/-2
 110 MPa16000 psiDry; ISO 527-1/-2
Elongation at Break 4.0 %4.0 %Dry; ISO 527-1/-2
 10 %10 %Conditioned; ISO 527-1/-2
Tensile Modulus 2.10 GPa305 ksiConditioned; ISO 527-1/-2
 5.40 GPa783 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C212 - 248 °FLong Term; ISO 2578
 220 °C428 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 60.0 °C140 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveInterior
Electricals & ElectronicsElectrical appliances
FormGranules
Industry & Consumer goodsHousewares
 Mechanical Engineering
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® TSGK-30 X PA666-(GF+GB)30
Celanese Nilit FRIANYL C73 HS-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced
Celanese Nilit FRIANYL C73 H-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced
Ashley Polymers Ashlene® 742L-33G Nylon 6/66, 33% Glass Reinforced
AlphaGary PVC 3016GBF-70S CLEAR 000X Polyvinyl Chloride Thermoplastic

PGRH280 / 156989

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.