MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Nilit FRIANYL C73 H-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Nylon 6.6/6 for injection molding, medium viscosity, heat stabilized.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Water Absorption 1.3 - 2.3 %1.3 - 2.3 %ISO 62
Water Absorption at Saturation 5.0 - 6.0 %5.0 - 6.0 %ISO 62
Viscosity Measurement 155155Viscosity index; ISO 307
Linear Mold Shrinkage 0.0040 - 0.012 cm/cm0.0040 - 0.012 in/inFRISETTA Test Method
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 170 MPa24700 psiISO 2039-1
Tensile Strength at Break 160 MPa23200 psiISO 527
Elongation at Break 2.5 %2.5 %ISO 527
Tensile Modulus 10.0 GPa1450 ksiISO 527
Flexural Strength 220 MPa31900 psiISO 178
Flexural Modulus 8.50 GPa1230 ksiISO 178
Charpy Impact Unnotched 2.50 J/cm²11.9 ft-lb/in²DIN 53453
 2.40 J/cm²
@Temperature -40.0 °C
11.4 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²DIN 53453
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 93
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 550 V550 VCTI 100; IEC 112
 
Thermal PropertiesMetricEnglishComments
Melting Point 242 °C468 °FISO 3146 DSC
Maximum Service Temperature, Air 120 °C248 °FContinuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 180 °C356 °FISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® HTNFR52G30BL NC010 PA6T/66-GF30FR(16+72)
Celanese Zytel® 74G33W NC010 PA66+PA6-GF33
Celanese Zytel® 74G33W BK196 PA66+PA6-GF33
Celanese Nilit FRIANYL C73 HS-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced
Ashley Polymers Ashlene® 742L-33G Nylon 6/66, 33% Glass Reinforced

PFRI193 / 39114

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.