MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Polymers 370 Polystyrene, High Heat
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Data provided by American Polymers, Inc. A high heat polystyrene produced in pellet form. It has excellent strength and clarity as well as fast set-up properties. Used in the manufacture of toys, containers, housewares, and medical applications. Processing methods include blow molding, extrusion and injection molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D892
Melt Flow 2.0 g/10 min2.0 g/10 minCondition G; ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 50.7 MPa7350 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 2.60 GPa377 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FAnnealed; ASTM D648
Vicat Softening Point 104 °C219 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Polymers API 375 Polystyrene
American Polymers API 650-21 Polystyrene
Overview of materials for Polystyrene, Molded, Unreinforced
Americas Styrenics EA3130 High Heat Crystal Polystyrene
Aclo Accucomp Polystyrene HS0600L High Impact

PAMER0 / 24001

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.