MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 2170T Flexible Plastic Bonder
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 2170T is a flexible, high viscosity, thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or almost any thermoplastic substrate. TRA-BOND 2170T is easy to apply and has an easy 1:1 mix ratio and can be cured at room temperature. This high technology system was formulated for applications in the automotive, medical, aerospace, photonic and assembly industries and can be used anywhere that requires excellent chemical fastening to plastic parts.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
Viscosity 22000 cP
@Temperature 25.0 °C
22000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565
Adhesive Bond Strength 17.2 MPa2500 psiLap shear, alum to alum
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 115 °C239 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 65.0 °C
1.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 120 min120 min
 
Descriptive Properties
Color Amber
Mix Ratio, parts by weight100/100Resin/Hardener
Thixotropic Index 4.55 rpm/50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Stycast® 2850FT-FR/11 Two-Component Epoxy Flame Retardant Encapsulant
Mocom (ALBIS) ALTECH® PA66 A 1000/517.01 IM Nylon 66
Taiwan Sheen Soon Sheenthane® AS-626SL TPU for PU Adhesive
Taiwan Sheen Soon Sheenthane® AH-701 TPU for Hotmelt Adhesive
SunChemical Gwent C2010517D4 Carbon/Graphite Ink

PTRAC056 / 70984

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.