MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ 7082 Carbon Conductor
Categories: Carbon

Material Notes: This product is a high resistivity conductor that can be used as a resistor. It was designed for applications requiring small resistance changes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³
Solids Content 28 - 32 %28 - 32 %
Particle Size 1.0 µm1.0 µm
Viscosity 210000 - 260000 cP210000 - 260000 cP
Thickness 7.00 - 14.0 microns0.276 - 0.551 mil
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1000 ohm1000 ohm
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hour
 
Descriptive Properties
AdhesionNo Material Transfer
Binder SystemProprietary
Conductive Filler TypeOther
Material TypeReady-To-Use Formulation
Recommended SubstratesPolyester
Solvent SystemEthylene glycol diacetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ 3571 Blend Member Dielectric
DuPont™ 5064 Silver Conductor
Aluminum 1350-H14
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Tetracalcium-Phosphate, Ca4PO9

PFLEXCM08 / 179410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.