MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ 5064 Silver Conductor
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: DuPont 5064 is one of several printed silver conductors, it can be printed with manual, semi-automatic, and reel-to-reel screen print equipment. The DuPont 5064 offers the lowest resistivity of any silver conductor commercially available today, thus providing a more cost effective solution than products requiring a thicker print to achieve final resistance values.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 63 - 66 %63 - 66 %
Filler Content 0.00 %0.00 %Silver (Ag)
Particle Size 1.0 µm1.0 µm
Viscosity 10000 - 20000 cP10000 - 20000 cP
Thickness 8.00 - 10.0 microns0.315 - 0.394 mil
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.0060 - 0.010 ohm0.0060 - 0.010 ohm
 
Processing PropertiesMetricEnglishComments
Cure Time 2.00 - 10.0 min0.0333 - 0.167 hour
 
Descriptive Properties
AdhesionNo Ag transfer after 3M Scotch Tape #600
Binder SystemProprietary
Conductive Filler TypeSilver (Ag)
Material TypeReady-To-Use Formulation
Recommended SubstratesPolyester, Paper, Card
Solvent SystemDiBasic Esters

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ 3571 Blend Member Dielectric
DuPont™ 7082 Carbon Conductor
Ovation Polymers Nemcon™ H PA DP117/X3 Polyphthalamide, Thermally Conductive
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant
DuPont™ 5018 UV Curable Dielectric

PFLEXCM69 / 179471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.