MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 610, Glass Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.14 - 1.66 g/cc0.0412 - 0.0600 lb/in³Average value: 1.35 g/cc Grade Count:97
Filler Content 15.0 - 50.0 %15.0 - 50.0 %Average value: 29.7 % Grade Count:33
Water Absorption 0.100 - 4.00 %0.100 - 4.00 %Average value: 1.23 % Grade Count:46
Moisture Absorption at Equilibrium 0.500 - 1.30 %0.500 - 1.30 %Average value: 0.935 % Grade Count:27
 0.900 - 1.50 %
@Temperature 70.0 - 70.0 °C
0.900 - 1.50 %
@Temperature 158 - 158 °F
Average value: 1.21 % Grade Count:16
Water Absorption at Saturation 0.350 - 2.40 %0.350 - 2.40 %Average value: 1.50 % Grade Count:10
 0.400 - 1.20 %
@Temperature 45.0 - 400 °C
0.400 - 1.20 %
@Temperature 113 - 752 °F
Average value: 0.814 % Grade Count:2
 0.400 - 1.20 %
@Treatment Temp. 70.0 - 70.0 °C
0.400 - 1.20 %
@Treatment Temp. 158 - 158 °F
Average value: 0.814 % Grade Count:2
Additive Loading 10.0 - 40.0 %10.0 - 40.0 %Average value: 24.5 % Grade Count:4
Viscosity Test 150 cm³/g1.50 dl/gAverage value: 150 cm³/g Grade Count:8
Linear Mold Shrinkage 0.00100 - 0.0510 cm/cm0.00100 - 0.0510 in/inAverage value: 0.00529 cm/cm Grade Count:80
Linear Mold Shrinkage, Transverse 0.00300 - 0.0790 cm/cm0.00300 - 0.0790 in/inAverage value: 0.0143 cm/cm Grade Count:48
Melt Flow 5.00 - 39.3 g/10 min5.00 - 39.3 g/10 minAverage value: 30.5 g/10 min Grade Count:10
Spiral Flow 35.0 - 45.0 cm13.8 - 17.7 inAverage value: 41.3 cm Grade Count:8
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118 - 120118 - 120Average value: 119 Grade Count:9
Ball Indentation Hardness 120 - 245 MPa17400 - 35500 psiAverage value: 183 MPa Grade Count:12
Tensile Strength, Ultimate 72.0 - 1330 MPa10400 - 193000 psiAverage value: 157 MPa Grade Count:89
 70.0 - 155 MPa
@Temperature 60.0 - 150 °C
10200 - 22500 psi
@Temperature 140 - 302 °F
Average value: 108 MPa Grade Count:2
Tensile Strength, Yield 138 - 193 MPa20000 - 28000 psiAverage value: 160 MPa Grade Count:11
Elongation at Break 2.00 - 25.0 %2.00 - 25.0 %Average value: 5.04 % Grade Count:85
 3.30 - 6.10 %
@Temperature 60.0 - 150 °C
3.30 - 6.10 %
@Temperature 140 - 302 °F
Average value: 4.59 % Grade Count:2
Elongation at Yield 2.50 - 6.00 %2.50 - 6.00 %Average value: 3.82 % Grade Count:19
Modulus of Elasticity 3.50 - 19.0 GPa508 - 2760 ksiAverage value: 9.23 GPa Grade Count:85
 3.00 - 9.80 GPa
@Temperature 60.0 - 150 °C
435 - 1420 ksi
@Temperature 140 - 302 °F
Average value: 5.86 GPa Grade Count:2
Flexural Yield Strength 121 - 340 MPa17500 - 49300 psiAverage value: 226 MPa Grade Count:58
Flexural Modulus 3.45 - 17.0 GPa500 - 2470 ksiAverage value: 8.51 GPa Grade Count:63
Flexural Strain at Break 3.60 - 5.50 %3.60 - 5.50 %Average value: 5.09 % Grade Count:6
Compressive Yield Strength 123 - 179 MPa17800 - 26000 psiAverage value: 155 MPa Grade Count:5
Poissons Ratio 0.340 - 0.3800.340 - 0.380Average value: 0.350 Grade Count:3
Izod Impact, Notched 0.534 - 1.87 J/cm1.00 - 3.50 ft-lb/inAverage value: 1.28 J/cm Grade Count:36
Izod Impact, Unnotched 4.27 - 13.7 J/cm8.00 - 25.7 ft-lb/inAverage value: 9.52 J/cm Grade Count:24
Izod Impact, Notched (ISO) 9.70 - 18.0 kJ/m²4.62 - 8.57 ft-lb/in²Average value: 14.7 kJ/m² Grade Count:6
 12.0 - 13.0 kJ/m²
@Temperature -40.0 - -30.0 °C
5.71 - 6.19 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 12.5 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 65.0 - 95.0 kJ/m²30.9 - 45.2 ft-lb/in²Average value: 78.7 kJ/m² Grade Count:5
Charpy Impact Unnotched 6.50 - 11.0 J/cm²30.9 - 52.4 ft-lb/in²Average value: 9.09 J/cm² Grade Count:54
 6.00 - 12.5 J/cm²
@Temperature -40.0 - -30.0 °C
28.6 - 59.5 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 8.96 J/cm² Grade Count:34
Charpy Impact, Notched 0.500 - 2.00 J/cm²2.38 - 9.52 ft-lb/in²Average value: 1.46 J/cm² Grade Count:43
 0.500 - 2.50 J/cm²
@Temperature -40.0 - -30.0 °C
2.38 - 11.9 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 1.17 J/cm² Grade Count:33
Falling Dart Impact 8.50 - 11.8 J6.27 - 8.70 ft-lbAverage value: 9.88 J Grade Count:4
Instrumented Impact Total Energy 2.72 - 4.76 J2.01 - 3.51 ft-lbAverage value: 3.55 J Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 100 - 1.00e+16 ohm-cm100 - 1.00e+16 ohm-cmAverage value: 8.84e+14 ohm-cm Grade Count:31
Surface Resistance 1000 - 1.00e+12 ohm1000 - 1.00e+12 ohmAverage value: 2.08e+11 ohm Grade Count:12
Dielectric Constant 3.70 - 3.803.70 - 3.80Average value: 3.75 Grade Count:4
Dielectric Strength 5.00 - 45.0 kV/mm127 - 1140 kV/inAverage value: 33.2 kV/mm Grade Count:15
Dissipation Factor 0.0140 - 0.01600.0140 - 0.0160Average value: 0.0153 Grade Count:3
Comparative Tracking Index 450 - 600 V450 - 600 VAverage value: 579 V Grade Count:12
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.3 - 48.6 µm/m-°C8.50 - 27.0 µin/in-°FAverage value: 25.7 µm/m-°C Grade Count:20
CTE, linear, Transverse to Flow 72.0 - 124 µm/m-°C40.0 - 68.9 µin/in-°FAverage value: 93.5 µm/m-°C Grade Count:11
Thermal Conductivity 0.476 - 0.562 W/m-K3.30 - 3.90 BTU-in/hr-ft²-°FAverage value: 0.531 W/m-K Grade Count:3
Melting Point 214 - 260 °C418 - 500 °FAverage value: 222 °C Grade Count:58
Maximum Service Temperature, Air 100 - 170 °C212 - 338 °FAverage value: 136 °C Grade Count:9
Deflection Temperature at 0.46 MPa (66 psi) 205 - 224 °C401 - 435 °FAverage value: 219 °C Grade Count:29
Deflection Temperature at 1.8 MPa (264 psi) 190 - 220 °C374 - 428 °FAverage value: 206 °C Grade Count:65
Deflection Temperature at 8.0 MPa 75.0 - 190 °C167 - 374 °FAverage value: 136 °C Grade Count:20
Vicat Softening Point 215 - 221 °C419 - 430 °FAverage value: 219 °C Grade Count:9
Glass Transition Temp, Tg 49.0 - 60.0 °C120 - 140 °FAverage value: 52.0 °C Grade Count:3
Flammability, UL94 HB - V-0HB - V-0Grade Count:52
 
Processing PropertiesMetricEnglishComments
Processing Temperature 274 - 293 °C525 - 560 °FAverage value: 284 °C Grade Count:9
Nozzle Temperature 240 - 305 °C464 - 581 °FAverage value: 270 °C Grade Count:8
Melt Temperature 50.0 - 310 °C122 - 590 °FAverage value: 267 °C Grade Count:52
Mold Temperature 8.00 - 120 °C46.4 - 248 °FAverage value: 84.4 °C Grade Count:58
Drying Temperature 70.0 - 90.0 °C158 - 194 °FAverage value: 80.1 °C Grade Count:36
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.164 % Grade Count:25
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:10
Injection Pressure 68.9 - 130 MPa10000 - 18900 psiAverage value: 96.7 MPa Grade Count:20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 610, Carbon Fiber Filled
Overview of materials for Nylon 610
Overview of materials for Nylon 63, 35% Glass-Filled
Overview of materials for Nylon 11, Unreinforced
Overview of materials for Nylon 46, Unreinforced

O2591 / 78043

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.