MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Potters Industries SHERIGLASS® Type VIII Solid Glass Spacer Bead
Categories: Ceramic; Glass

Material Notes: Potters Industries LLC offers specialized glass beads specifically designed for controlling bond line thickness in adhesive bonding. These beads are manufactured and certified to meet the specification requirements of Raytheon HMS20-1776 and Boeing SCGMS-53004.

Information provided by Potters Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.30 - 2.70 g/cc0.0831 - 0.0975 lb/in³
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.50 - 1.551.50 - 1.55
 
Descriptive Properties
ColorColorless
Diameter0.0035 in
Magnetic Iron<0.1%
Sieve0.0029-0.0035 inASTM D1214, 90% of Product Within Diameter Range
 170 microns100% Passes
 200 microns90-100% Passes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott N-LASF31a Glass
Poraver Idealboard (2-4 mm), various applications with high strength
Poraver Carrier-panel (0.25-0.5 mm), Sandwich panel, Work plate
Poraver Acoustic-panel (0.5-1 mm), Structural, Engineering
Corning 7761 Potash Borosilicate Crushed/Powdered Glass

CPOT8058 / 184684

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.