MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poraver Idealboard (2-4 mm), various applications with high strength
Categories: Ceramic; Glass

Material Notes: The low weight of Poraver® in combination with high compressive strength and its excellent compatibility with polyurethane generates plenty of innovative applications in many different industrial sectors. Aside from the cost reduction a high stiffness at low densities is achieved through the use of Poraver®.

Properties:

  • Improvement of stiffness to weight ratio
  • low density of 300 gk/m3 possible with every low thermal conductivity of 0.08 W/m-K
  • no change of strength after heat-resistance-test (shortly up to 250°C)
  • no extension of the panels
  • open porous, breathable
  • humidity resistant
  • high compressive strength
  • high screw withdrawal resistance
Advanced board properties achievable in combination with:
  • glass fiber mats
  • grid textiles
  • silicone plasters
  • fire retarding agents
  • façade protection coating

Information provided by Poraver®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.280 - 0.349 g/cc0.0101 - 0.0126 lb/in³
Particle Mesh Size 5.0 - 10 Mesh5.0 - 10 Mesh
Thickness 2000 - 4000 microns78.7 - 157 milGranular
 15200 - 61000 microns600 - 2400 mil
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 6.00 - 8.00 MPa870 - 1160 psi
 
Descriptive Properties
Screw-Withdrawal Resistance108-600 lbf

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott N-LASF31a Glass
Potters Industries SHERIGLASS® Type VIII Solid Glass Spacer Bead
Poraver Carrier-panel (0.25-0.5 mm), Sandwich panel, Work plate
Poraver Acoustic-panel (0.5-1 mm), Structural, Engineering
Corning 7761 Potash Borosilicate Crushed/Powdered Glass

CPOR016 / 186905

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.