MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch-Weld™ FLX300 Flexible Instant Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: 3M™ Scotch-Weld™ Flexible Instant Adhesive FLX (formerly PR851) is formulated for extended resistance to impact, vibration, stress, peel, and humidity applications. It is faster curing than 3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Brookfield Viscosity 200 - 400 cP200 - 400 cPLVF Spindle #2 @ 30 rpm
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 20.0 MPa2900 psiOverlap; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 71.0 °C160 °F
Minimum Service Temperature, Air -54.0 °C-65.2 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.167 - 0.583 min0.00278 - 0.00972 hourTime to Handling Strength
 1440 min24.0 hourFull Cure
 
Descriptive Properties
AppearanceClear liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parson Adhesives PARFIX® 3496 Cyanoacrylate Adhesive
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy

PMM34692 / 169439

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.