MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay CYCOM® 977-6 Epoxy Prepreg Laminate with T300 Plain Weave Fabric
Categories: Polymer; Thermoset; Epoxy

Material Notes: Cycom® 977-6 is a tough lower temperature curing modified epoxy resin. It is a versatile curing toughened epoxy resin which can be cured from 135°C to 177°C, depending on service temperature requirements. Following a 177°C cure, 977-6 has a 138°C dry and a 104°C wet service temperature. Cycom® 977-6 is formulated for lower temperature autoclave or press mold processing. Typical applications for Cycom® 977-6 include high performance automotive, aircraft primary and secondary structure, space structure, and any application where impact resistance and lightweight as well as versatile cure conditions are required.

Features & Benefits:

  • Toughened epoxy uses “co-continuous” morphology.
  • Very high impact resistance. CSAI up to 40ksi.
  • Controlled flow.
  • Tg of ~150°C following 3hr @ 135°C cure. (DMA G’)
  • Excellent cured surface finish.
  • 14 days shop life.
  • 12 months shelf life at -18°C
  • Available in a wide range of fibers and fabric weaves.
Property data for laminate with T300 Plain Weave Fabric 50%-1KT300-p-120-1000

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³
Outgassing - Total Mass Loss 0.070 %0.070 %WVR; ASTM E595
 0.13 %0.13 %TML; ASTM E595
Collected Volatile Condensable Material 0.00 %0.00 %ASTM E595
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1230 MPa179000 psiActual 50%VF
 1360 MPa197000 psiNormalized 55% VF
Tensile Modulus 80.0 GPa11600 ksiActual 50%VF
 88.0 GPa12800 ksiNormalized 55% VF
Compressive Strength 766 MPa111000 psiActual 50%VF
 841 MPa122000 psiNormalized 55% VF
Compressive Modulus 70.0 GPa10200 ksiActual 50%VF
 77.0 GPa11200 ksiNormalized 55% VF
Shear Strength 82.7 MPa12000 psiInterlaminar, Actual 42.7% VF
 88.9 MPa12900 psiInterlaminar, Actual 50%VF
 139 MPa20200 psiIn Plane, Actual 42.7% VF
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 104 °C219 °FWet
 138 °C280 °FDry
Glass Transition Temp, Tg 165 °C329 °FRDS DMA, 5°C/min, G'
 173 °C343 °FRDS DMA, 5°C/min, G"
 185 °C365 °FRDS DMA, 5°C/min, Tan d
 
Processing PropertiesMetricEnglishComments
Processing Temperature 135 - 180 °C275 - 356 °FCure Temp
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay LTM® 26EL Epoxy with T300 Woven Carbon Fiber Laminate
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber
Solvay EF1812 Polycarbosilane Polymer, Pyrolized with T300 Carbon Fabric
Park Aerospace Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced
Park Aerospace Nelcote® E-765 Epoxy Prepreg, T300 3K PW Reinforced

PCYTED135_7 / 192715

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.