MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teijin Multilon TN-7000 Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It is a typical type with high flowability, light resistance and heat stability that is suitable for a business machine chassis etc..

Information provided by Teijin Chemicals Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Thickness 4.00 mm
0.0040 - 0.0060 in/in
@Thickness 0.157 in
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 4.00 mm
0.0040 - 0.0060 in/in
@Thickness 0.157 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.0 MPa6960 psi50mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa9140 psi50mm/min; ISO 527
Elongation at Break 80 %80 %50mm/min; ISO 527
Elongation at Yield 3.0 %3.0 %50mm/min; ISO 527
Flexural Strength 95.0 MPa13800 psi2mm/min; ISO 178
Flexural Modulus 2.60 GPa377 ksi2mm/min; ISO 178
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
ISO 11359
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C183 °FISO 75
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 5VA
@Thickness 2.00 mm
5VA
@Thickness 0.0787 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teijin Multilon TN-7500 Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Teijin Multilon TN-7100F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Teijin Multilon T-2711 Standard, Automobile Part Series PC/ABS Polymer Alloy
Teijin Multilon T-3011 Standard PC/ABS Polymer Alloy
Teijin Multilon TN-7000F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy

PTEIJ45 / 69734

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.