MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teijin Multilon T-2711 Standard, Automobile Part Series PC/ABS Polymer Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PC/ABS polymer alloy general grade developed for automobile parts use. It has high heat resistance, impact strength, light resistance and fluidity, particularly, the high impact strength in a wide range from -30 to over 100. Therefore, it is getting good estimation in a plurality of applications as automobile parts. Higher fluidity and thermal stability enable various processings such as, a gas-assist molding, hot-runner molding and compression molding.

Applications:

  • Car interior components (cluster, panels etc.)
  • Audio and car-navigation equipment parts etc.
  • Information provided by Teijin Chemicals Ltd.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.14 g/cc0.0412 lb/in³ISO 1183
    Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
    @Thickness 4.00 mm
    0.0050 - 0.0070 in/in
    @Thickness 0.157 in
    Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
    @Thickness 4.00 mm
    0.0050 - 0.0070 in/in
    @Thickness 0.157 in
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength at Break 48.0 MPa6960 psi50mm/min; ISO 527
    Tensile Strength, Yield 56.0 MPa8120 psi50mm/min; ISO 527
    Elongation at Break 110 %110 %50mm/min; ISO 527
    Elongation at Yield 3.0 %3.0 %50mm/min; ISO 527
    Tensile Modulus 2.25 GPa326 ksi1mm/min; ISO 527
    Flexural Strength 85.0 MPa12300 psi2mm/min; ISO 178
    Flexural Modulus 2.30 GPa334 ksi2mm/min; ISO 178
    Charpy Impact Unnotched NBNBISO 179
    Charpy Impact, Notched 8.00 J/cm²38.1 ft-lb/in²ISO 179
     
    Electrical PropertiesMetricEnglishComments
    Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear 80.0 µm/m-°C
    @Temperature 20.0 °C
    44.4 µin/in-°F
    @Temperature 68.0 °F
    ISO 11359
    CTE, linear, Transverse to Flow 80.0 µm/m-°C
    @Temperature 20.0 °C
    44.4 µin/in-°F
    @Temperature 68.0 °F
    ISO 11359
    Deflection Temperature at 0.46 MPa (66 psi) 124 °C255 °FISO 75
    Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FISO 75
    Vicat Softening Point 122 °C252 °F50°C/hr, 50N; ISO 306

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Teijin Multilon DN-1530B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
    Teijin Multilon TN-7100F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
    Teijin Multilon DN-3510F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
    Teijin Multilon DN-3520F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
    Mitsubishi Iupilon® MB 2212R PC/ABS

    PTEIJ44 / 69733

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.