MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Murtfeldt Muralen® plus + AB Polyethylene, Antibacterial
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of its great cut, impact, and shock resistance, this material is often used to make underlays for cutting and punching machines and for ram guards.

Special Properties:
• High cut resistance
• Good shock and impact absorption
• Good resistance to chemicals
• Good anti-adhesion properties
• Approved for use in the food industry (EU and FDA)
• Good weldability
• Antibacterial properties

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: PE-HMW
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density <= 0.950 g/cc<= 0.0343 lb/in³ISO 1183
Moisture Absorption at Equilibrium <= 0.10 %<= 0.10 %ISO 62
Water Absorption at Saturation <= 0.10 %<= 0.10 %ISO 62
Molecular Weight 500000 g/mol500000 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666DIN 53505
Ball Indentation Hardness 45.0 MPa6530 psi
Tensile Strength 27.2 MPa3950 psiISO 527
Tensile Strength, Yield 20.0 MPa2900 psiISO 527
Elongation at Break 630 %630 %ISO 527
Modulus of Elasticity 1.10 GPa160 ksi
Compressive Yield Strength  9.00 MPa
@Strain 1 %
1310 psi
@Strain 1 %
ISO 604
 15.0 MPa
@Strain 2 %
2180 psi
@Strain 2 %
ISO 604
 23.0 MPa
@Strain 5.0 %
3340 psi
@Strain 5.0 %
ISO 604
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched >= 2.50 J/cm²>= 11.9 ft-lb/in²ISO 179
Coefficient of Friction, Dynamic 0.180.18
Sand Slurry 350350value in %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
Dielectric Constant  2.4
@Frequency 100 Hz
2.4
@Frequency 100 Hz
IEC 60250
 2.4
@Frequency 1e+6 Hz
2.4
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength <= 45.0 kV/mm<= 1140 kV/inIEC 60243
Dielectric Loss Index  0.00020
@Frequency 100 Hz
0.00020
@Frequency 100 Hz
IEC 60250
 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C
@Temperature 23.0 - 60.0 °C
111 µin/in-°F
@Temperature 73.4 - 140 °F
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FISO 52612
Melting Point 130 - 135 °C266 - 275 °FISO 3146
Maximum Service Temperature, Air 80.0 °C
@Time 1.80e+7 sec
176 °F
@Time 5000 hour
Minimum Service Temperature, Air -100 °C-148 °F
Glass Transition Temp, Tg -120 °C-184 °F
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
European Food 1935/2004 YesYes
FDA YesYes
 
Descriptive Properties
ColorSky Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial
American Elements Z-MITE™ Zinc Oxide Nanopowder
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Aclo Accutech Polyethylene HD0234G20UVL High Density Glass Reinforced UV Stabilized

PMURT918 / 156565

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.