MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro DESMODUR® MD1380 + BAYTEC® D21 + BAYTEC® XL B (Catalyst SD2-40) 75A Polyurethane, MDI-Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccBAYTEC® XL B
 1.13 g/cc1.13 g/ccBAYTEC® D21
 1.15 g/cc1.15 g/ccDESMODUR® MD1380
 1.21 g/cc1.21 g/cc
Viscosity 30 cP30 cPBAYTEC® XL B
 1100 cP1100 cPBAYTEC® D21
 1200 cP1200 cPDESMODUR® MD1380
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575DIN 53505
 72
@Temperature 80.0 °C
72
@Temperature 176 °F
DIN 53505
 78
@Temperature -5.00 °C
78
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 27.0 MPa3920 psiDIN 53504
Tensile Stress at Strain 1.20 MPa
@Strain 10 %
174 psi
@Strain 10 %
DIN 53504
Elongation at Break 500 %500 %DIN 53504
100% Modulus 4.50 MPa
@Strain 100 %
653 psi
@Strain 100 %
DIN 53504
200% Modulus 6.00 MPa
@Strain 200 %
870 psi
@Strain 200 %
DIN 53504
300% Modulus 8.00 MPa
@Strain 300 %
1160 psi
@Strain 300 %
DIN 53504
Resilience 4848[%]; DIN 53512
Tear Strength 28.9 kN/m165 pliwith nick; ISO 34-1
 84.0 kN/m479 pliwithout nick; ISO 34-1
Abrasion 3535[mm3]; ISO 4649
Compression Set 24 %
@Temperature 70.0 °C,
Time 79200 sec
24 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 45.0 °C113 °FBAYTEC® XL B
 60.0 °C140 °FBAYTEC® D21
 80.0 °C176 °FDESMODUR® MD1380
Mold Temperature 110 °C230 °F
Pot Life 2.00 min2.00 min
 
Descriptive Properties
AppearancesolidDESMODUR® MD1380
 solidBAYTEC® D21
 solidBAYTEC® XL B
Content0.11SD2-40 % / total (by weight), (catalyst at the head)
 100Parts by weight of prepolymer
 2.1SD2-40 % / BAYTEC® XL B (by weight), to mix with BAYTEC® XL B
 30Parts by weight of BAYTEC® D21
 7.4Parts by weight of BAYTEC® XL B
 8.35-8.75%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMOPHEN® C 1100 Polyurethane
Lubrizol LifeSciences Tecothane® Soft AR-75A TPU
Lubrizol Estane® 2355-75A Thermoplastic Polyurethane Elastomer
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A, with 0.35 phr CAYTUR 4
Covestro Acclaim® 3300N Polyol

PCOVEST0404 / 202187

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.