MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMODUR® MD1380 + BAYTEC® D21 + BAYTEC® XL B (Catalyst SD2-40) 75A Polyurethane, MDI-Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccBAYTEC® XL B
 1.13 g/ccBAYTEC® D21
 1.15 g/ccDESMODUR® MD1380
 1.21 g/cc
Viscosity 30 cPBAYTEC® XL B
 1100 cPBAYTEC® D21
 1200 cPDESMODUR® MD1380
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75DIN 53505
 72
@Temperature 80.0 °C
DIN 53505
 78
@Temperature -5.00 °C
DIN 53505
Tensile Strength at Break 27.0 MPaDIN 53504
Tensile Stress at Strain 1.20 MPa
@Strain 10 %
DIN 53504
Elongation at Break 500 %DIN 53504
100% Modulus 0.00450 GPa
@Strain 100 %
DIN 53504
200% Modulus 0.00600 GPa
@Strain 200 %
DIN 53504
300% Modulus 0.00800 GPa
@Strain 300 %
DIN 53504
Resilience 48[%]; DIN 53512
Tear Strength 165 pliwith nick; ISO 34-1
 479 pliwithout nick; ISO 34-1
Abrasion 35[mm3]; ISO 4649
Compression Set 24 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815-1
 
Processing PropertiesOriginal ValueComments
Processing Temperature 45.0 °CBAYTEC® XL B
 60.0 °CBAYTEC® D21
 80.0 °CDESMODUR® MD1380
Mold Temperature 110 °C
Pot Life 2.00 min
 
Descriptive Properties
AppearancesolidDESMODUR® MD1380
 solidBAYTEC® D21
 solidBAYTEC® XL B
Content0.11SD2-40 % / total (by weight), (catalyst at the head)
 100Parts by weight of prepolymer
 2.1SD2-40 % / BAYTEC® XL B (by weight), to mix with BAYTEC® XL B
 30Parts by weight of BAYTEC® D21
 7.4Parts by weight of BAYTEC® XL B
 8.35-8.75%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMOPHEN® C 1100 Polyurethane
Lubrizol LifeSciences Tecothane® Soft AR-75A TPU
Lubrizol Estane® 2355-75A Thermoplastic Polyurethane Elastomer
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A, with 0.35 phr CAYTUR 4
Covestro Acclaim® 3300N Polyol

PCOVEST0404 / 202187

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.