MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Magnesium
Magnesium Elektron - Service & Innovation in Magnesium

Magnesium Elektron Elektron® AZ91E Magnesium Casting Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: ELEKTRON AZ91E is a general purpose gravity sand casting alloy containing aluminum, zinc and manganese. Good properties may be achieved particularly with the use of chills in the mold. Corrosion resistance is excellent.

Applications: The alloy may be used in aerospace casting applications particularly where there is no high temperature requirement or a requirement for pressure tightness.

Information provided by Magnesium Elektron.

Key Words: ASTM B80 AZ91E; BS2970 MAG7/3; DIN MgAl /19 Zn1; AFNOR G-A9Z1; BS2L125; ISO 16220 MC21120
Vendors: Magnesium Elektron is the world leader in high strength magnesium alloys in rolled, extruded and cast forms. Phone (303) 589-3189 or visit www.magnesium-elektron.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.81 g/cc1.81 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7575
Tensile Strength at Break >= 117 MPa>= 17000 psiMin Design Specification per ASTM B80 AZ91E; T6 condition
 260 MPa37700 psiTypical, T4
 270 MPa39200 psiTypical, T6
Tensile Strength, Yield  >= 83.0 MPa
@Strain 0.2 %
>= 12000 psi
@Strain 0.2 %
Min Design Specification per ASTM B80 AZ91E; T6 condition
 125 MPa
@Strain 0.2 %
18100 psi
@Strain 0.2 %
Typical, T4
 170 MPa
@Strain 0.2 %
24700 psi
@Strain 0.2 %
Typical, T6
Elongation at Break >= 2.0 %>= 2.0 %Min Design Specification per ASTM B80 AZ91E; T6 condition
 4.5 %4.5 %Typical, T6
 9.0 %9.0 %Typical, T4
Modulus of Elasticity 44.0 GPa6380 ksi
Compressive Yield Strength 130 MPa
@Strain 0.2 %
18900 psi
@Strain 0.2 %
Compressive Strength 400 MPa58000 psi
Poissons Ratio 0.350.35
Fatigue Strength 70.0 MPa
@# of Cycles 5.00e+7
10200 psi
@# of Cycles 5.00e+7
Rotating Bend
Fracture Toughness 13.2 MPa-m½12.0 ksi-in½KIC
Shear Strength 140 MPa20300 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000141 ohm-cm0.0000141 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 27.0 µm/m-°C15.0 µin/in-°F
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°F
Thermal Conductivity 84.0 W/m-K583 BTU-in/hr-ft²-°F
Melting Point 470 - 595 °C878 - 1100 °F
Solidus 470 °C878 °F
Liquidus 595 °C1100 °F
Shrinkage 1.3 %1.3 %Pattern Makers Shrinkage Factor
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.1 - 9.3 %8.1 - 9.3 %
Magnesium, Mg 89.35 - 91.33 %89.35 - 91.33 %As Balance
Manganese, Mn 0.17 - 0.35 %0.17 - 0.35 %
Zinc, Zn 0.40 - 1.0 %0.40 - 1.0 %
 
Descriptive Properties
Corrosion rate<50 mpyASTM B117 Salt spray test
Damping Index0.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium Elektron Elektron® AZ31B Magnesium Extrusion Alloy, UNS M11311
Magnesium Elektron Elektron® ZRE1 Magnesium Alloy, UNS M12330
Magnesium Elektron Elektron® 43 Magnesium Extrusion Alloy, UNS M18434
Magnesium Elektron Elektron® W28 Magnesium Alloy Welding Rod Composition
Magnesium Elektron Elektron® W7 Magnesium Alloy Welding Rod Composition

NMAGEL901 / 186916

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.