MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyimide, Graphite Filled
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.33 - 1.67 g/cc0.0480 - 0.0603 lb/in³Average value: 1.49 g/cc Grade Count:49
Filler Content 10.0 - 40.0 %10.0 - 40.0 %Average value: 21.7 % Grade Count:13
Water Absorption 0.0800 - 2.00 %0.0800 - 2.00 %Average value: 0.539 % Grade Count:33
 0.530 - 3.15 %
@Temperature 50.0 - 80.0 °C
0.530 - 3.15 %
@Temperature 122 - 176 °F
Average value: 1.73 % Grade Count:10
 0.380 - 2.18 %
@Temperature 80.0 - 80.0 °C
0.380 - 2.18 %
@Temperature 176 - 176 °F
Average value: 1.73 % Grade Count:5
 0.380 - 2.18 %
@Time 86400 - 86400 sec
0.380 - 2.18 %
@Time 24.0 - 24.0 hour
Average value: 1.73 % Grade Count:5
Water Absorption at Saturation 1.00 - 3.40 %1.00 - 3.40 %Average value: 1.98 % Grade Count:6
 2.30 - 2.30 %
@Temperature 80.0 - 80.0 °C
2.30 - 2.30 %
@Temperature 176 - 176 °F
Average value: 2.30 % Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 75.0 - 11975.0 - 119Average value: 98.6 Grade Count:12
Hardness, Shore D 78.0 - 90.078.0 - 90.0Average value: 84.1 Grade Count:28
Tensile Strength, Ultimate 35.0 - 146 MPa5080 - 21200 psiAverage value: 74.7 MPa Grade Count:42
 23.0 - 52.0 MPa
@Temperature 250 - 260 °C
3340 - 7540 psi
@Temperature 482 - 500 °F
Average value: 32.7 MPa Grade Count:6
Tensile Strength, Yield 63.0 - 101 MPa9140 - 14600 psiAverage value: 77.9 MPa Grade Count:8
Elongation at Break 1.00 - 10.0 %1.00 - 10.0 %Average value: 3.25 % Grade Count:43
 2.00 - 9.80 %
@Temperature 260 - 260 °C
2.00 - 9.80 %
@Temperature 500 - 500 °F
Average value: 5.55 % Grade Count:4
Modulus of Elasticity 2.65 - 8.58 GPa384 - 1240 ksiAverage value: 4.62 GPa Grade Count:32
Flexural Yield Strength 55.0 - 229 MPa7980 - 33200 psiAverage value: 109 MPa Grade Count:44
 31.0 - 63.4318 MPa
@Temperature 250 - 260 °C
4500 - 9200.02 psi
@Temperature 482 - 500 °F
Average value: 46.2 MPa Grade Count:6
Flexural Modulus 2.74 - 8.02 GPa397 - 1160 ksiAverage value: 4.53 GPa Grade Count:34
 1.86 - 5.17 GPa
@Temperature 250 - 260 °C
270 - 750 ksi
@Temperature 482 - 500 °F
Average value: 2.87 GPa Grade Count:6
Flexural Strain at Break 1.30 - 5.50 %1.30 - 5.50 %Average value: 3.15 % Grade Count:7
Flexural Strain at Yield 1.40 - 4.60 %1.40 - 4.60 %Average value: 3.12 % Grade Count:13
Compressive Strain at Break 12.0 - 30.0 %12.0 - 30.0 %Average value: 19.0 % Grade Count:3
Compressive Yield Strength 25.0 - 466 MPa3630 - 67600 psiAverage value: 147 MPa Grade Count:35
Compressive Modulus 0.847 - 7.94 GPa123 - 1150 ksiAverage value: 3.27 GPa Grade Count:21
Izod Impact, Notched 0.135 - 0.507 J/cm0.253 - 0.950 ft-lb/inAverage value: 0.308 J/cm Grade Count:10
Charpy Impact Unnotched 0.700 - 4.60 J/cm²3.33 - 21.9 ft-lb/in²Average value: 2.26 J/cm² Grade Count:19
Charpy Impact, Notched 0.110 - 0.480 J/cm²0.524 - 2.28 ft-lb/in²Average value: 0.250 J/cm² Grade Count:26
Coefficient of Friction 0.200 - 0.3000.200 - 0.300Average value: 0.250 Grade Count:5
Compression Set 12.5 - 50.4 %12.5 - 50.4 %Average value: 31.1 % Grade Count:11
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 3.00e+6 - 4.00e+19 ohm-cm3.00e+6 - 4.00e+19 ohm-cmAverage value: 4.45e+18 ohm-cm Grade Count:9
Surface Resistance 1000 - 1.00e+15 ohm1000 - 1.00e+15 ohmAverage value: 8.82e+13 ohm Grade Count:16
Dielectric Constant 3.30 - 62.03.30 - 62.0Average value: 15.6 Grade Count:8
Dielectric Strength 3.00 - 33.0 kV/mm76.2 - 838 kV/inAverage value: 14.9 kV/mm Grade Count:9
Dissipation Factor 0.00130 - 0.3100.00130 - 0.310Average value: 0.0469 Grade Count:7
Comparative Tracking Index 175 - 399 V175 - 399 VAverage value: 295 V Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.0 - 63.0 µm/m-°C6.11 - 35.0 µin/in-°FAverage value: 37.7 µm/m-°C Grade Count:16
 15.0 - 97.0 µm/m-°C
@Temperature 50.0 - 400 °C
8.33 - 53.9 µin/in-°F
@Temperature 122 - 752 °F
Average value: 43.2 µm/m-°C Grade Count:19
Specific Heat Capacity 0.970 - 1.13 J/g-°C0.232 - 0.270 BTU/lb-°FAverage value: 1.04 J/g-°C Grade Count:6
Thermal Conductivity 0.317 - 4.47 W/m-K2.20 - 31.0 BTU-in/hr-ft²-°FAverage value: 1.59 W/m-K Grade Count:22
 0.490 - 1.66 W/m-K
@Temperature 40.0 - 40.0 °C
3.40 - 11.5 BTU-in/hr-ft²-°F
@Temperature 104 - 104 °F
Average value: 0.893 W/m-K Grade Count:3
Maximum Service Temperature, Air 260 - 360 °C500 - 680 °FAverage value: 299 °C Grade Count:19
Deflection Temperature at 0.46 MPa (66 psi) 285 - 376 °C545 - 709 °FAverage value: 333 °C Grade Count:9
Deflection Temperature at 1.8 MPa (264 psi) 263 - 417 °C505 - 783 °FAverage value: 321 °C Grade Count:17
Minimum Service Temperature, Air -196 - -196 °C-321 - -321 °FAverage value: -196 °C Grade Count:7
Glass Transition Temp, Tg 260 - 397 °C500 - 747 °FAverage value: 328 °C Grade Count:26
UL RTI, Electrical 50.0 - 130 °C122 - 266 °FAverage value: 119 °C Grade Count:3
UL RTI, Mechanical with Impact 50.0 - 130 °C122 - 266 °FAverage value: 119 °C Grade Count:3
UL RTI, Mechanical without Impact 50.0 - 130 °C122 - 266 °FAverage value: 119 °C Grade Count:3
Flammability, UL94 V-0 - 5VAV-0 - 5VAGrade Count:16

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyimide
Overview of materials for Thermoplastic Polyimide, Unfilled
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
Overview of materials for Polyimide, Thermoset Film
Arkema KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion

O4207 / 78303

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.