MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sulfur Hexafluoride, SF6
Categories: Ceramic; Halide; Fluid

Material Notes: Colorless gas. Strong greenhouse gas, therefore its use is being severely restricted.

Key Words: SF6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.00597 g/cc0.000216 lb/in³Gas
Molecular Weight 146.055 g/mol146.055 g/mol
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility -0.0000440-0.0000440cm^3/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 34.4 J/g14.8 BTU/lb
Thermal Conductivity  0.00920 W/m-K
@Pressure 0.000 MPa,
Temperature -73.1 °C
0.0638 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature -99.7 °F
gas; low pressure limiting value
 0.0130 W/m-K
@Pressure 0.000 MPa,
Temperature 26.9 °C
0.0902 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 80.3 °F
gas; low pressure limiting value
 0.0206 W/m-K
@Pressure 0.000 MPa,
Temperature 127 °C
0.143 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 260 °F
gas; low pressure limiting value
 0.0275 W/m-K
@Pressure 0.000 MPa,
Temperature 227 °C
0.191 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 440 °F
gas; low pressure limiting value
 0.0338 W/m-K
@Pressure 0.000 MPa,
Temperature 327 °C
0.235 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 620 °F
gas; low pressure limiting value
Melting Point -50.7 °C-59.3 °Ftriple point
Boiling Point -63.8 °C-82.8 °F
 
Descriptive Properties
CAS Number2551-62-4

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Cast, Metal Filled
AISI Type H13 Hot Work Tool Steel
Hydrogen Bromide, HBr
Titanium Ti-6Al-4V (Grade 5), Annealed
Chlorine, Cl2

EINOR0784 / 3918

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.