MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chlorine, Cl2
Categories: Fluid; Pure Element

Key Words: Chlorine, Cl2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.002898 g/cc0.0001047 lb/in³Gas
Molecular Weight 70.905 g/mol70.905 g/mol
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 35.452735.45271995
Atomic Number 1717
X-ray Absorption Edge 4.3969 Å4.3969 ÅK
 52.084 Å52.084 ÅLI
 61.366 Å61.366 ÅLII
 61.672 Å61.672 ÅLIII
Critical Temperature 143.8 °C290.8 °F
Critical Molar Volume 123 cm³/mol7.51 in³/mol
Electronegativity 3.163.16Pauling
Ionic Radius 0.270 Å0.270 ÅCrystal Ionic Radius for Valence +7
 0.340 Å0.340 ÅCrystal Ionic Radius for Valence +5
 1.81 Å1.81 ÅCrystal Ionic Radius for Valence -1
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 90.26 J/g38.83 BTU/lb
Heat of Vaporization 287.8 J/g123.8 BTU/lbAt Boiling Point
 247.7 J/g
@Temperature 25.0 °C
106.6 BTU/lb
@Temperature 77.0 °F
Specific Heat Capacity 0.476 J/g-°C0.114 BTU/lb-°F
Melting Point -101.5 °C-150.7 °F
Boiling Point -34.04 °C-29.27 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molGas
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.3834
@Temperature 20.0 °C,
Wavelength 589 nm
1.3834
@Temperature 68.0 °F,
Wavelength 589 nm
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 100 %100 %
 
Descriptive Properties
AppearanceGreen-Yellow Gas
CAS Number7782-50-5

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Argon, Ar
Fluorine, F2
Neon, Ne
Bromine, Br2
Overview of materials for Polypropylene, Extrusion Grade

AMECl / 21

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.