MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips HiD® 9606 HDPE Blown Film and Sheet  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Resin Type: ASTM D 4976 Classification: PE 235, A 54502

Applications:General Purpose Films and Sheet, Coextruded Film Structures, Deli and Tissue Films, Sheet Thermoforming Applications with Good Stress Crack Resistance

Film properties below based on film thickness of 25.4 µm.

Data provided by Chevron Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc0.0344 lb/in³ASTM D1505
Melt Flow 0.26 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.26 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
High Load Melt Index 30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
30 g/10 min
@Load 47.6 lb,
Temperature 374 °F
High Load Melt Index; ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 530 %530 %ASTM D882
Film Elongation at Break, TD 400 %400 %ASTM D882
Secant Modulus, MD 0.750 GPa109 ksiASTM D882
Secant Modulus, TD 0.910 GPa132 ksiASTM D882
Elmendorf Tear Strength, MD 0.394 g/micron10.0 g/milNotched; ASTM D1922
Elmendorf Tear Strength, TD 4.33 g/micron110 g/milASTM D1922
Dart Drop <= 1.20 g/micron<= 30.5 g/milF50; 1.5 in. dart/26 in. drop height; ASTM D 1709
Film Tensile Strength at Break, MD 28.0 MPa4060 psiASTM D882
Film Tensile Strength at Break, TD 21.0 MPa3050 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 126 °C259 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 221 °C430 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
FKuR Kunststoff Bio-Flex® F 6514 PLA Blend
Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene
Elix Polymers Elix™ H604 ABS Polymer
Elix Polymers ELIX™ 112H Acrylonitrile Butadiene Styrene (ABS)
Eastman M2001-P Polyethylene

PCHEVV64 / 20460

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.