MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elix Polymers ELIX™ 112H Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: High Heat ABS copolymer modified with alpha-methylstyrene-SAN used to impart superior Heat Distortion resistance for PVC & ABS resin.

Typical applications: Can be applied in PVC compounds (e.g. calendered films, sheets, siding, profiles) and ABS resin; Major benefits might include :

  • increased thermal resistance (dimensional stability and service temperature)
  • superior melt strength and emboss retention for thermoformed parts
  • improved toughness in PVC compounds
Chemical composition: ABS copolymer modified with alpha-methylstyrene-SAN.

Physical form: White to slightly yellow powder

Information provided by Elix Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.380 - 0.480 g/cc0.0137 - 0.0173 lb/in³ASTM D1895
Particle Size 125 - 500 µm125 - 500 µm>90%; ASTM D1921
Melt Flow 2.5 - 6.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
2.5 - 6.5 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point >= 112 °C
@Load 12.2 kg
>= 234 °F
@Load 27.0 lb
B50; ISO 306
 
Descriptive Properties
Content<0.2%Residual monomers
 12.8-15.5%Polybutadiene
Hardness Hc30>100 MPaISO 2039-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Denka TH-11 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
Denka TE-20 Transparent Resin Polymer (MABS resin) ABS
Cossa Polimeri ESTALUX 5513 Methyl Methacrylate Acrylonitrile Butadiene Styrene
FKuR Kunststoff Bio-Flex® F 6514 PLA Blend
Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene

PELIX032 / 183347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.