MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik TEGOMER® AntiScratch 200 Polyamide compound
Categories: Polymer

Material Notes: Product description: TEGOMER® AntiScratch 200 is a siloxane polyamide compound delivered in pelletized form.

Application:

  • TEGOMER® AntiScratch 200 is recommended to be used in polyamide compounds and other engineered polymers to guarantee permanent scratch resistance
  • TEGOMER® AntiScratch 200 should be used with up to 4 % in filled PA systems. The higher the filler content the higher the dosage level of TEGOMER® AntiScratch 200 has to be.
  • TEGOMER® AntiScratch 200 can be applied in polyamide co-compounds with non-polar thermoplastic materials such as PP.
  • TEGOMER® AntiScratch 200 will enhance glass fiber filled PA compounds regarding melt flow and by that brilliant appearance of dark surfaces occurs.
Benefits: TEGOMER® AntiScratch 200 is a non-migrating additive for the improvement of permanent, long-term scratch resistance. TEGOMER® AntiScratch 200 can be used in com-pounding or molding operations. TEGOMER® AntiScratch 200 works in a wide range of talc or glass fibre filled systems, which are used for automotive or E&E applications. TEGOMER® AntiScratch 200 does not influence the gloss of the polyamide compound. TEGOMER® AntiScratch 200 is suitable for thermoplastic polyamides which are compounded with other thermoplastic polymers. TEGOMER® AntiScratch 200 reduces, due to better melt flow, the cutting of glass fibers during com-pounding. Therefore, moulded parts show less melt flow lines and a more brilliant black or coloured appearance.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.270 - 0.370 g/cc0.00975 - 0.0134 lb/in³
 
Descriptive Properties
Appearancewhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGOMER® P 121 Dispersing additive
Evonik TEGO® SMO 80 V Emulsifier
Evonik TEGOMER® DA 800 Dispersing additive
Avient OnFlex™ S FR 50A-3S1831 Thermoplastic Elastomer (TPE)
Barlog Plastics KEBAFLEX U A 75 ST B01 natural TPU, Shore A75, natural

PEVONIL573 / 196777

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.