Product description: TEGOMER® DA 800 is a non-ionic, modified fatty acid derivative. Application: TEGOMER® DA 800 is a liquid dispersing additive used for pigment concentrates for the production of: - Liquid color pastes which might be either water-based for water-based systems or oil-based to be used for the liquid coloration of thermoplastic polymers instead of solid concentrates.
- Pastes of inorganic fillers, carbon blacks and organic pigments
- Solid masterbatches: if the material is applied with a gravimetric side feeding or in low concentration also at the typical feeding position (just 5 parts of 100 parts formulation).
Benefits: - Universally suitable for inorganic and organic pigments
The use of TEGOMER® DA 800 offers several ad-vantages of a dispersant for the production of pigment concentrates:- Excellent color strength development
- Enables low viscosity liquid pigment concentrates
- No yellowing of bright colored finishes or plastic parts due to high temperature resistance
- Solvent, amine and nonylphenol ethoxylate-free
- Suitable as continuous phase for liquid pastes
Information provided by Evonik |