MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: PA 6/66

The Durethan® product line was transferred to Envalior, but this product was discontinued prior to that transaction.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.027 g/cc1.027 g/ccISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.0 MPa4060 psiISO 527-1,-2
Elongation at Yield 6.5 %6.5 %ISO 527-1,-2
Tensile Modulus 0.210 GPa30.5 ksiConditioned; ISO 527-1,-2
 0.980 GPa142 ksiISO 527-1,-2
Flexural Strength  12.0 MPa
@Strain 9.0 %
1740 psi
@Strain 9.0 %
Conditioned; ISO 178
 35.0 MPa
@Strain 6.1 %
5080 psi
@Strain 6.1 %
ISO 178
Flexural Yield Strength  7.00 MPa
@Strain 3.5 %
1020 psi
@Strain 3.5 %
Conditioned; ISO 178
 30.0 MPa
@Strain 3.5 %
4350 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 0.230 GPa33.4 ksiConditioned; ISO 178
 0.980 GPa142 ksiISO 178
Izod Impact, Notched (ISO)  85.0 kJ/m²
@Temperature -30.0 °C
40.4 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 90.0 kJ/m²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO) NBNBISO 180-1U
Charpy Impact, Notched 10.5 J/cm²
@Temperature -30.0 °C
50.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 200 µm/m-°C111 µin/in-°FISO 11359-1,-2
CTE, linear, Transverse to Flow 200 µm/m-°C111 µin/in-°FISO 11359-1,-2
Melting Point 211 °C412 °FISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 53.0 °C127 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C118 °FISO 75-1,-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 280 °C446 - 536 °FRecommended
 270 °C518 °FProcessing conditions for test specimens; ISO 294
Mold Temperature 60.0 - 90.0 °C140 - 194 °FRecommended
 80.0 °C176 °FProcessing conditions for test specimens; ISO 294
Drying Temperature 80.0 °C176 °F
Dry Time 2 - 6 hour2 - 6 hour
Moisture Content 0.00 - 0.060 %0.00 - 0.060 %Residual; Acc. To Karl Fischer
 
Descriptive Properties
ISO Short NameISO 1874-PA 6/66-HI,BHS,14-010

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6
Domo TECHNYL® B 230 PA66/6, DRY
Ashley Polymers Ashlene® 747 Nylon 6/66
EMS-Grivory Grilon® TSGL-60/4 black 9833 PA666-GF60
EMS-Grivory Grilon® TS V0 PA666

PLANX0936 / 120761

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.