MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: PA 6/66

The Durethan® product line was transferred to Envalior, but this product was discontinued prior to that transaction.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.027 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 28.0 MPaISO 527-1,-2
Elongation at Yield 6.5 %ISO 527-1,-2
Tensile Modulus 210 MPaConditioned; ISO 527-1,-2
 980 MPaISO 527-1,-2
Flexural Strength 12.0 MPa
@Strain 9.0 %
Conditioned; ISO 178
 35.0 MPa
@Strain 6.1 %
ISO 178
Flexural Yield Strength 7.00 MPa
@Strain 3.5 %
Conditioned; ISO 178
 30.0 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 230 MPaConditioned; ISO 178
 980 MPaISO 178
Izod Impact, Notched (ISO) 85.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 90.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) NBISO 180-1U
Charpy Impact, Notched 105 kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 200 µm/m-°CISO 11359-1,-2
CTE, linear, Transverse to Flow 200 µm/m-°CISO 11359-1,-2
Melting Point 211 °CISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 53.0 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °CISO 75-1,-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 280 °CRecommended
 270 °CProcessing conditions for test specimens; ISO 294
Mold Temperature 60.0 - 90.0 °CRecommended
 80.0 °CProcessing conditions for test specimens; ISO 294
Drying Temperature 80.0 °C
Dry Time 2 - 6 hour
Moisture Content 0.00 - 0.060 %Residual; Acc. To Karl Fischer
 
Descriptive Properties
ISO Short NameISO 1874-PA 6/66-HI,BHS,14-010

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6
Domo TECHNYL® B 230 PA66/6, DRY
Ashley Polymers Ashlene® 747 Nylon 6/66
EMS-Grivory Grilon® TSGL-60/4 black 9833 PA666-GF60
EMS-Grivory Grilon® TS V0 PA666

PLANX0936 / 120761

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.