Microtherm® Board is a high performance thermal insulation made at a lower density than normal Microtherm products. The insulation is an opacified blend of filament reinforced pyrogenic silica, specifically blended for toughness and optimized manipulation.Properties- Low density high temperature thermal insulation
- Stable thermal performance for continuous exposure to 1000°C (1832°F)
- Excellent machineability
- Non combustible
- Environmentally safe
- Free of harmful respirable fibers
Applications- Thermal batteries - rapid heat up
- Space and Aerospace - lower weight
- Portable fuel cells - easier to carry
- Furnaces - easy installation
Information provided by Microtherm. |