MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Westlake EBAC® SP2810 16% EBA copolymer
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: EBAC® SP2810 is a 16% EBA copolymer designed for blown film, co-extrusions, and blends where flexibility and strength are important. SP2810 provides excellent elasticity and low temperature performance and can be used to improve the performance of various polymers and bitumen/asphalt blends. EBAC® resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVC, unplasticized PVC and other polar polymers. For use as heat seal layer, adhesive layer, or modifiers for cost/performance enhancement. They are soft, pliable and tough at ambient and freezing temperatures and exhibit excellent ESCR. These polymers exhibit high solids fillability and compatibility with a wide range of polymers. This facilitates their use as bases for all-purpose concentrates. Thermal stability allows processing like LDPE. This product has some 21 CFR clearances. Key Attributes: Compatibility with various polymers, Good heat and RF sealing, Low temperature toughness, Soft, flexible, and tough without plasticizers. Application/Uses: Films, Flexible Packaging, Asphalt Modification, Impact Modification, Wire and Cable.

Samples tested at 23°C and 50% RH.

Information provided by Westlake Chemical Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D1505
Butyl Acrylate Content 16 %16 %
Melt Index of Compound 1.4 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545ASTM D2240
Tensile Strength at Break 10.3 MPa1500 psi500 mm/min; ASTM D638 TYPE IV
Tensile Strength, Yield 12.4 MPa1800 psi500mm/min; ASTM D638 TYPE IV
Elongation at Break 600 %600 %500mm/min, Type IV specimen; ASTM D638
Modulus of Elasticity 0.0827 GPa12.0 ksiType IV specimen; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 96.0 °C205 °FDSC Peak; ASTM D3418
Vicat Softening Point 67.0 °C153 °FASTM D1525
Brittleness Temperature <= -73.0 °C<= -99.4 °FASTM D 746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake EMAC® SA2413 Ethylene Methyl Acrylate Copolymer
LyondellBasell Lucalen A2920M Low Density Polyethylene
Westlake EBAC® Plus SP1903 18% Ethylene Butyl Acrylate Copolymer
Westlake EBAC® SP1802 22.5% Ethylene Butyl Acrylate Copolymer
Westlake EBAC® SP1806 17.5%, Ethylene-Methyl Acrylate Copolymer

PWESF8812 / 222884

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.