MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

KiON HTT 1800  (discontinued **)
Categories: Fluid; Polymer; Thermoset

Material Notes: KiON HTT 1800 is a pale yellow, low viscosity liquid polysilazane-based coating resin that is specially designed for use in the formulation of heat-curable ceramic coatings capable of withstanding operating temperatures of 1800°F or above. KiON HTT 1800 is supplied as a 100% “solids” liquid of low viscosity, and rapidly solidifies upon heating to 350-400°F. KiON HTT 1800 can be blended with a variety of pigments, such as metal powders (zinc, aluminum, stainless steel), ceramic powders (silicon carbide, aluminum oxide, silicon nitride), or the like. For ultra-high temperature formulations, the coated part is then heated to at least 850°F to promote conversion of the polymer to ceramic. Depending on the exact formulation, coating operating temperatures of 1800°F or above can be achieved.

Applications

High Temperature Coatings and Thermally Stable Corrosion Coatings

Information provided by KiON, A Clariant Business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³Liquid
Viscosity 80 cP
@Temperature 19.0 °C
80 cP
@Temperature 66.2 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point 29.0 °C84.2 °F
 
Descriptive Properties
%Resin100% solids as liquid
AppearanceClear to pale yellow liquid

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
KiON CERASET® POLYSILAZANE 20 (PSZ 20)
KiON CERASET® POLYUREASILIZANE 20 (PURS 20)
3M Techical Ceramics Ekatherm® Silicon Nitride
Inhance Fluoro-Seal INHANCE® Si-8220 Polymer Alloy
Inhance Fluoro-Seal INHANCE® Si-8500 Polymer Alloy

PKION05 / 48721

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.