MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Inhance Fluoro-Seal INHANCE® Si-8500 Polymer Alloy
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: INHANCE S i-8000 series polymer alloy consists of black, medium density, silicon carbide chemically modified for greater adhesion. This product was designed for alloying with various polymer materials such as epoxy, polyurea, polyurethane etc. When incorporated in polymers, unique grades of high-performance polymeric composites are formed that have exceptional abrasion-resistance and wear performance. Frequently these composites have abrasion resistance greater than metal. They are also are light weight, non-corroding, and electrically non-conductive.

Applications: Ideal applications include wear resistant parts that can be molded for severe service in mechanical or chemical environments, where repair/replacement of worn parts is very costly because of down time, and where optimal performance is needed. Examples include belt wipers, mining components, impact resistant products, screens, dumping pads, chute liners, valve seats, piston rings, gears, wear-plates, guide-rails, cable (protective jacketing), steel replacement parts, and high performance coatings.

Information provided by Inhance/Fluoro-Seal, Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.20 g/cc3.20 g/cc
Bulk Density 1.28 g/cc0.0462 lb/in³
Particle Size 25 µm25 µmaverage
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 24502450

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Inhance Fluoro-Seal INHANCE® Ti--9113 Titanium Carbide Polymer Alloy
Inhance Fluoro-Seal INHANCE® Si-8220 Polymer Alloy
Inhance Fluoro-Seal INHANCE® Ti-9100 Titanium Carbide Polymer Alloy
Inhance Fluoro-Seal INHANCE® Ti-9000 Titanium Carbide
Inhance Fluoro-Seal INHANCE® UH-1250 Ultra High Molecular Weight Polyethylene

PINHAN015 / 137226

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.