MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Eastman Amphora™ AM1800 3D Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Eastman Amphora™ 3D polymer is a low-odor, styrene-free choice that is uniquely suited for 3D printing applications. With Amphora, makers can create items that are more functional, durable, efficient, and attractive. Now you can fulfill your vision with 3D creations that exhibit excellent aesthetics and superior toughness. Amphora also complies with certain U.S. Food and Drug Administration (FDA) regulations for food contact applications. That means, with Amphora, you’ll be able to make a lot of things you can’t with other materials. Best of all, you’ll be able to make certain your final product meets your expectations.

Applications/Uses:

  • Production of 3D Printing filaments
Key Attributes:
  • Clarity and gloss
  • Dimensional stability
  • Ease of processing
  • Enhanced aesthetics
  • Excellent toughness and temperature resistance
  • FDA compliance
  • Low odor
  • Property retention in 3D applications
  • Styrene-free
  • Workability

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength at Break 28.0 MPa4060 psiASTM D638
Tensile Strength, Yield 50.0 MPa7250 psiASTM D638
Elongation at Break 110 %110 %ASTM D638
Elongation at Yield 5 %5 %ASTM D638
Tensile Modulus 1.90 GPa276 ksiASTM D638
Flexural Modulus 2.10 GPa305 ksiASTM D790
Izod Impact, Notched 0.930 J/cm
@Temperature 23.0 °C
1.74 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Manufacturer mentions clarity but doesn't quantify
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 °C473 °F
 
Descriptive Properties
Processing - CoolingAs needed up to 100%
Processing - Heated Bed 70°C (158°F)
Processing - Infill50-90%
Processing - Layer Height0.2 mm
Processing - Perimeter1.2 mm
Processing - Speed30-60 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tritan™ EX401 Copolyester
Resirene Resirene® 6110 High Impact Polystyrene
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin
Akro-Plastic Akromid® A3 GF 25 (2420) PA 6.6 Conditioned, 25% Glass Filled
3D Systems QuickPlastic Cast Urethane Material ABSLike

PE8930 / 176030

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.