System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Resirene Resirene® 6110 High Impact Polystyrene
Categories:
Polymer
;
Thermoplastic
;
Polystyrene (PS)
;
Polystyrene, Impact Modified
Material Notes:
Features:
High Impact
Easy Processing
FDA Rating: 21 CFR 177.1640
Flexibility
Applications:
Injection Molding
TV Cabinets
Remote Controls
Toys
Information provided by US distributor Calsak Corporation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.04
g/cc
1.04
g/cc
ASTM D792
Linear Mold Shrinkage
0.0030
-
0.0070
cm/cm
0.0030
-
0.0070
in/in
ASTM D955
Melt Flow
10
g/10 min
@Load 5.00 kg,
Temperature 200 °C
10
g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
12.4
MPa
1800
psi
ASTM D638
Tensile Strength, Yield
15.9
MPa
2310
psi
ASTM D638
Elongation at Break
50 %
50 %
ASTM D638
Tensile Modulus
2.034
GPa
295.0
ksi
ASTM D638
Izod Impact, Notched
1.04
J/cm
1.95
ft-lb/in
0.5 in.; ASTM D256
1.23
J/cm
2.30
ft-lb/in
0.125 in.; ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
72.0
°C
162
°F
ASTM D648
Flammability, UL94
HB
HB
Compliance Properties
Metric
English
Comments
FDA
Yes
Yes
See notes for details.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Eastman Amphora™ AM1800 3D Polymer
Akro-Plastic Akromid® A3 GF 25 (2420) PA 6.6 Conditioned, 25% Glass Filled
Plastics Group Polifil® RP-HIPS High Impact Polystyrene
Overview of materials for Nylon 46, Glass Fiber Reinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
PRESIR10 / 65552
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.