MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

Saint-Gobain Meldin® 7022 DF Direct Formed Graphite Filled Polyimide
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: Melidin® 7022 DF is a direct formed polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin® 7000 series polyimide.

Specification Qualifications:
Satisfies Type II, Class 2D for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide Resin
Satisfies Class 3, Form D for SAE AMS 3644G: Polyimide, Molded Rod, Bar and Tube, Plaque, and Formed Parts
Satisfies Type II, Class 2D for MIL-R-46198: Resin, Polyimide, Hot Pressed or Pressed and Sintered

Information provided by Saint-Gobain Performance Plastics

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³ASTM D792
Deformation 0.15 %0.15 %2000 psi load; ASTM D621
 <= 0.0020 %
@Temperature 260 °C
<= 0.0020 %
@Temperature 500 °F
ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  27.6 MPa
@Temperature 260 °C
4000 psi
@Temperature 500 °F
ASTM D638
 49.6 MPa
@Temperature 23.0 °C
7200 psi
@Temperature 73.4 °F
ASTM D638
Elongation at Break  3.0 %
@Temperature 23.9 °C
3.0 %
@Temperature 75.0 °F
ASTM D638
 3.0 %
@Temperature 260 °C
3.0 %
@Temperature 500 °F
ASTM D638
Flexural Strength  41.4 MPa
@Temperature 260 °C
6000 psi
@Temperature 500 °F
ASTM D790
 72.4 MPa
@Temperature 23.9 °C
10500 psi
@Temperature 75.0 °F
ASTM D790
Flexural Modulus  2.60 GPa
@Temperature 260 °C
377 ksi
@Temperature 500 °F
ASTM D790
 4.50 GPa
@Temperature 23.9 °C
653 ksi
@Temperature 75.0 °F
ASTM D790
Compressive Yield Strength  22.8 MPa
@Strain 1 %
3300 psi
@Strain 1 %
ASTM D695
 96.5 MPa
@Strain 10 %
14000 psi
@Strain 10 %
ASTM D695
Compressive Modulus 2.00 GPa290 ksiASTM D695
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.8 µm/m-°C
@Temperature 22.8 - 260 °C
11.0 µin/in-°F
@Temperature 73.0 - 500 °F
ASTM E831

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
7022 Aluminum Composition Spec
7020-T6 Aluminum
Constellium Certal® Thick Aluminum Plate
Manifattura Cattaneo VESPEL® SP21 Polyimide
DuPont Mobility and Materials Vespel® SCP-5050 Polyimide

PSTGQZ085 / 150623

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.