MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient OnForce™ LFT NY-50LGF/001 HS Natural Polyamide 6 (Nylon 6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. These products exhibit enhanced physical and mechanical properties versus standard short fiber products. Benefits of LFT compounds include improved impact strength, elastic modulus, and material strength across wide temperature ranges from subambient to highly elevated. Furthermore, LFT compounds have been shown to offer improved performance in the areas of creep and fatigue performance, improved dimensional stability, and exhibit an exceptional surface finish when compared to traditional highly filled short fiber products.

LFT compounds can be processed using equipment similar to that used for short fiber products. The mechanical properties of finished parts depend greatly on the length of the fibers in the molded part; therefore processing conditions must be set carefully in order to minimize fiber breakage. A low shear process is advised, with low back pressure, low screw speed and low-to-medium injection speed.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 g/cc0.0571 lb/in³ISO 1183
Filler Content 50 %50 %Long Glass Fiber
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inMeasured on a tensile specimen.; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 200 MPa29000 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Tensile Modulus 14.5 GPa2100 ksiISO 527-2
Flexural Strength 290 MPa42100 psiISO 178
Flexural Modulus 13.5 GPa1960 ksiISO 178
Charpy Impact Unnotched 7.50 J/cm²35.7 ft-lb/in²ISO 179
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²ISO 179
Gardner Impact 14.1 J10.4 ft-lbASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 212 °C414 °FUnannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 188 °C370 °FUnannealed; ISO 75-2/C
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 90.0 °C194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour
Back Pressure 1.00 MPa145 psi
 
Descriptive Properties
FeaturesHeat Stabilized
FormsPellets
Generic MaterialNylon 6
Generic NamePolyamide 6 (Nylon 6)
Injection RateSlow-Moderate
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Latamid 6 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized
Domo TechnylStar™ SX 216 V50 PA6, 50% glass filled, DRY
Domo TechnylStar™ SX 216 V50 PA6, 50% glass filled, Conditioned
Envalior Durethan® BKV 50 H2.0 EF 000000 Nylon 6, 50% Glass Fiber
Envalior Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber

PH0POL1420 / 145989

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.