MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmodur® XP 2619 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Desmodur XP 2619 is an aromatic isocyanate based on diphenylmethane diisocyanate.

Properties / Applications: Desmodur XP 2619 may be used in combination with suitable Desmophen® grades in the formulation of solvent-free, two-pack polyurethane coatings, fillers, sealing compounds and synthetic resin mortars. It is necessary to add water scavengers such as molecular sieve paste 3 Å to the polyol component to prevent the undesired reaction of Desmodur XP 2619 with water. Systems formulated with Desmodur XP 2619 are suitable for coating concrete, asphalt, fibrous cement and plastics. As with any product, use of Desmodur XP 2619 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/cc
Solids Content 100 %100 %
Viscosity 130 cP130 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 198 °C388 °F
 
Descriptive Properties
Content31-32.5%Isocyanate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODURE® N 3900 Polyurethane
Covestro DESMODURE® N 3800 Polyurethane
Covestro DESMODURE® N 3790 BA Polyurethane
Covestro DESMODURE® N 3600 Polyurethane
Covestro DESMODURE® N 3400 Polyurethane

PCOVEST0674 / 202457

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.